Applications
Lightly Doped Single Crystalline Diamond BDD SCD
Single-crystal & Monosectorial
Orientation of face surfaces: (100)
Surface roughness, Ra ≈ 5 nm
Miscut from the {100} surface: +/-3.0°
Parallelism: +/- 0.05 mm
Lateral Tolerance: +/- 0.05 mm
Thickness tolerance: +/- 0.05 mm
Edges: laser cut and polished
Dimensional tolerance at corners: <0.02 mm,
Boron concentration: ≈1 ppm